T8铝灯头
| 171R-111 | ||||
| 产品特性及应用 | ||||
| 性能 Property |
测试标准 Standard Test |
测试条件 Test Condition |
单位 Unit | 数值 Value |
| 机械性能 Mechanical Properties |
||||
| 拉伸强度 Tensile Strength@Yield |
D638 | 50mm/min | Mpa | 68 |
| 断裂伸长率 Elongation at Break |
D638 | 50mm/min | % | 120 |
| 弯曲强度 Flexural Yield Strength |
D790 | 10mm/min | Mpa | 75 |
| 弯曲模量 Flexural Modulus |
D790 | 10mm/min | Mpa | 2,480 |
| 缺口冲击强度 Izod Impact, Notched |
D256 | 1/8",23℃ | J/m | 700 |
| D256 | 1/8",-40℃ | J/m | - | |
| 物理性能 Physical Properties |
||||
| 熔融指数 Melt Flow |
D1238 | 300℃,1.2kg | g/10min | 12-16 |
| 成型收缩率 Linear Mold Shrinkage |
D955 | % | 0.5-0.7 | |
| 密度 Density |
D792 | 23℃ | g/cc | 1.2 |
| 热性能 Thermal Properties |
||||
| 热变形温度 heat deflection temperature |
D648 | 0.46MPa | ℃ | |
| D648 | 1.82MPa | ℃ | 120 | |
| 阻燃性能 flammability |
UL94 | 1.5mm | Class | V0 |
| 电性能 Electrical Properties |
||||
| 体积电阻 Volume Resistivity |
D 257 | ohm-cm | 1E+15 | |
| 加工工艺 Processing |
||||
| 干燥温度 Drying Temperature |
℃ | 100~120 | ||
| 干燥时间 Drying Time |
hrs | 4~5 | ||
| 料筒温度 Cylinder Temperature |
℃ | 260~280 | ||
| 模具温度 Mold Temperature |
℃ | 110~120 | ||
| * 以上数值是根据实验标准测定的代表数值。因为本资料是根据本公司实验数据所作成,所以这些数据未必适用各种不同的条件,最终还请客户自行作出判断。上述所列的仅是产品的基本信息而不是产品规格。 | ||||